Let s talk about the reason for the paint bulge after the solid wood door cover is painted

Updated on Solid wood 2024-06-20
1 answers
  1. Anonymous users2024-01-24

    This may be because the putty is not dry, the surface of the putty is not clean, and then you spray paint directly, he will bulge, it is recommended that you let him dry quickly, it is best to speed up the drying, and then redo the spray paint.

Related questions
1 answers2024-06-20

Hello, everyone thinks that solid wood doors are environmentally friendly, in fact, the paint of solid wood doors is also a source of pollution. Of course, if you choose a paint with an eco-friendly logo, you'll be fine.

2 answers2024-06-20

Yes, you have to remove it, and it depends on what kind of color you want to change. >>>More

2 answers2024-06-20

1. The wood board inside the paint is deformed and cracked, resulting in cracking of the external paint; Second, the putty is too thick or the paint itself is too thick, or the paint is not dry during construction, and the next layer is brushed, resulting in cracking. After finding out the cause of cracking, deal with the first situation separately: use No. 0 iron sand to grind off the paint surface, and wait for a period of time to make the moisture content of the board and wood normal. >>>More

4 answers2024-06-20

A set of paint can be brushed 60 squares at once. In the case of PU, 3 to 4 primers and 1 to 2 topcoats, in the case of NC, 1 to 2 primers and 6 to 7 topcoats are done for open, and for closed ones, the primer is more than a few times and the topcoat is less. >>>More

1 answers2024-06-20

The peeled paint film should be cleaned up, and then the oiler will repair the base layer and repaint it!