How to deal with solid wood furniture that is prone to cracking in autumn

Updated on Solid wood 2024-05-14
1 answers
  1. Anonymous users2024-01-23

    In autumn, when the temperature is dry, the moisture content of solid wood furniture will naturally decrease, which will cause cracking in the wood. So what should we do to solve this situation.

    Once the furniture is cracked, if it is not remedied in time, it is easy to cause a wide range of cracking problems, and once the solid wood furniture cracks, it becomes very ugly. At the same time, if the remediation is timely, the solid wood furniture can naturally be used for a longer time. How can it be remedied?

    First of all, cut the waste newspaper into paper scraps, then add alum and stir well, then pour in a small amount of water and mix well. Wait until you're about the same stirring, then cook the ingredients into a paste. Next, the boiled paste mixture is filled into the cracks of the solid wood furniture, allowed to air dry, and finally the filling area is painted with a furniture repair pen to harmonize the color of the entire furniture.

    Although the method introduced above is not simple, you can also try it. In addition to this method, in daily life, we also maintain solid wood furniture at all times to avoid premature cracking, such as decoration companies in the process of transporting solid wood furniture, we must be careful to carry it, remember to be light, stable and flat, and at the same time to stay away from heat sources, that is, too strong light. Finally, regular waxing and varnishing of solid wood furniture is also a good way to maintain it.

Related questions
1 answers2024-05-14

It is recommended to re-nail the interface, and if it does not work in the middle, you can use putty to fill it.

2 answers2024-05-14

Greasy with putty, make wood grain and then spray paint.

2 answers2024-05-14

Solid wood furniture retains the color of the original wood and can be brushed with varnish so that the surface is easy to clean!

1 answers2024-05-14

Preparation materials: 600 mesh sandpaper, 502 glue, wood wax oil trial pack or water-based wood paint (topcoat) trial pack, scraper, repair putty. >>>More

4 answers2024-05-14

In winter, the high temperature and dryness of the room cause the wood to shrink, but because the whole surface is fixed, the shrinkage force of the wood cannot be released, and eventually it cracks. >>>More